Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connectors and terminals.
Mechanical Properties
Round Wire
Annealed |
|
42 |
52 |
.0010 - .1285 inch |
1/4 Hard |
H01 |
57 |
72 |
1/2 Hard |
H02 |
73 |
88 |
3/4 Hard |
H03 |
85 |
100 |
Hard |
H04 |
95 |
110 |
Extra Hard |
H06 |
105 |
120 |
Spring |
H08 |
115 |
|
Square Wire
Annealed |
|
42 |
52 |
.0100 - .0808 inch |
1/4 Hard |
H01 |
57 |
72 |
1/2 Hard |
H02 |
73 |
88 |
3/4 Hard |
H03 |
85 |
100 |
Hard |
H04 |
95 |
110 |
Extra Hard |
H06 |
105 |
120 |
Spring |
H08 |
115 |
|
Rolled Flat
Annealed |
|
40 |
50 |
Thickness:
.0100 - .0500 inch
Width:
.0150 - .2500 inch
|
1/4 Half Hard |
H01 |
49 |
59 |
1/2 Hard |
H02 |
57 |
69 |
3/4 Hard |
H03 |
62 |
74 |
Hard |
H04 |
70 |
82 |
Extra Hard |
H06 |
76 |
88 |
Spring |
H08 |
84 |
94 |
Extra Spring |
H10 |
92 |
|
Physical Properties
Melting Point (Liquidis) |
1890°F |
Melting Point (Solidus) |
1850°F |
Density |
0.316 lbs/cu in |
Electrical Resistivity (Annealed) |
37 Ω⋅cmil/ft @ 68°F |
Electrical Conductivity (Annealed) |
28% IACS @ 68°F |
Thermal Conductivity (Solutionized-Aged) |
69 Btu ft/sq ft hr °F @ 68°F |
Coefficient of Thermal Expansion |
0.0000102°F (68-572°F) |
Modulus of Elasticity (Tension) |
16000 ksi |
Mechanical Properties
Round Wire
Annealed |
|
290 |
360 |
.0254 - 3.264 mm |
1/4 Hard |
H01 |
395 |
495 |
1/2 Hard |
H02 |
505 |
605 |
3/4 Hard |
H03 |
585 |
690 |
Hard |
H04 |
655 |
760 |
Extra Hard |
H06 |
725 |
825 |
Spring |
H08 |
795 |
0 |
Square Wire
Annealed |
|
290 |
360 |
.2540 - 1.905 mm |
1/4 Hard |
H01 |
395 |
495 |
1/2 Hard |
H02 |
505 |
605 |
3/4 Hard |
H03 |
585 |
690 |
Hard |
H04 |
655 |
760 |
Extra Hard |
H06 |
725 |
825 |
Spring |
H08 |
795 |
0 |
Rolled Flat
Annealed |
|
275 |
345 |
Thickness:
.2540 - 1.905 mm
Width:
.3810 - 6.350 mm
|
1/4 Half Hard |
H01 |
340 |
405 |
1/2 Hard |
H02 |
395 |
475 |
3/4 Hard |
H03 |
425 |
510 |
Hard |
H04 |
485 |
565 |
Extra Hard |
H06 |
525 |
605 |
Spring |
H08 |
580 |
650 |
Extra Spring |
H10 |
635 |
0 |
Physical Properties
Melting Point (Liquidis) |
1032°C |
Melting Point (Solidus) |
1010°C |
Density |
8.74696 gm/cu cm |
Electrical Resistivity (Annealed) |
6.151 ?? -cm @ 20°C |
Electrical Conductivity (Annealed) |
0.16392 MegaSiemens /cm @ 20°C |
Thermal Conductivity (Solutionized-Aged) |
119.4789 W/m · °K @ 20°C |
Coefficient of Thermal Expansion |
0.00001836°C (20-300°C) |
Modulus of Elasticity (Tension) |
110300 MPa |